Re: [Classicrendezvous] Restoring Anodization; Was:polishing NR/SR parts

(Example: Framebuilding:Tubing:Falck)

Date: Thu, 16 Nov 2000 11:08:53 +0000
From: Mark Stevens <m.stevens@camb.linst.ac.uk>
Organization: Camberwell College of Arts
To: PeterGrenader <peterg@ixpres.com>
CC: Cino1947@aol.com, classicrendezvous@bikelist.org
Subject: Re: [Classicrendezvous] Restoring Anodization; Was:polishing NR/SR parts
References: <5a.d02676c.2742057d@aol.com> <3A12A3F7.294E7E48@ixpres.com>


Hi All, I have access to a bead blaster here at college. It will strip anodizing at 120 psi to allow a high polish to be put on the aluminium . Then turn the pressure down to about 40 psi and with fresh beads you can replicate the dull sheen of anodizing. I have had great success on derailleurs and cranks.

Mark 'in flooded London 'Stevens